CA 1189701
ABSTRACT OF THE DISCLOSURE A high-concentration coal-water slurry of a coal concentration as high as 71 percent by weight at a viscosity of 2,000 cp (at 25°C) can be produced by first coarsely crushing a starting coal, further pul- verizing 95 to 30 percent by weight of the coarsely crushed thus obtained, subjecting the finely pulverized coal thus obtained, together with the remainder of the coarsely crushed coal, to crushing in a wet-type crusher, and pulverizing and adjusting the coal particles to a particle size constitution of 20 to 30 percent by weight of 200-mesh size and larger and 80 percent by weight or less of 350-mesh size and smaller.
416908
Itoh Hayami
Kamao Mitsugu
Nakaoji Kazuhiko
Takao Shoichi
Tatsumi Shuhei
Electric Power Development Company Limited
Fetherstonhaugh & Co.
Kao Corporation
Kawasaki Jukogyo Kabushiki Kaisha
Lion Corporation
LandOfFree
Process for producing high-concentration coal-water slurry does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing high-concentration coal-water slurry, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing high-concentration coal-water slurry will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1187547