CA 2126058

PROCESS FOR PRODUCING POLYCRYSTALLINE DENSE SHAPED BODIES BASED ON BORON CARBIDE BY PRESSURELESS SINTERING ABSTRACT OF THE DISCLOSURE A process for producing shaped bodies of boron carbide, metal diboride and carbon, which includes (a) homogeneously mixing pulverulent boron carbide with at least one pulverulent monocarbide of an element Ti, Zr, Hf, V, Nb and Ta in an amount corresponding to from 2% to 6% by weight of free carbon, based on the total weight of the boron carbide; (b) shaping this mixture into green bodies of a density of at least 50% TD; (c) heating the preformed body thus obtained to from about 1250°C to 1450°C with exclusion of oxygen in a sintering furnace and maintaining it within this temperature range for from 10 to 120 minutes; and (d) subsequently sintering the preformed body by heating to from 2100°C to 2250°C.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing polycrystalline dense shaped bodies... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing polycrystalline dense shaped bodies..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing polycrystalline dense shaped bodies... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1965819

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.