ABSTRACT OF THE DISCLOSURE Disclosed is a process for recovering valuable metals from scrap including the steps of melting the initial scrap feed, carburizing the melt, solidifying the carburized melt, and re- covering the valuable metals from the resultant material by an acid or ammoniacal leaching step.
320990
Cabot Corporation
Sherman
LandOfFree
Process for recovering valuable metals from superalloy scrap does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for recovering valuable metals from superalloy scrap, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for recovering valuable metals from superalloy scrap will most certainly appreciate the feedback.