Process for sintering aluminum nitride to a high thermal...

C - Chemistry – Metallurgy – 04 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C04B 35/64 (2006.01) C04B 35/581 (2006.01)

Patent

CA 2155836

Sintered aluminium nitride bodies having a TC of at least 200 W/m.K are prepared by sintering under non-reducing conditions and controlling interrelated parameters such as binder burnout atmosphere, heating rate, sintering temperature, time at sintering temperature, cooling rate and cooling temperature. The sintered bodies may also have a TC in excess of 270 W/m.K.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for sintering aluminum nitride to a high thermal... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for sintering aluminum nitride to a high thermal..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for sintering aluminum nitride to a high thermal... will most certainly appreciate the feedback.