ABSTRACT A process for the concentration of sulfidic nickel ores from basic rocks by means of froth flotation is described. The flotation reagent used is dithiophosphate with a pH of 3.5-6Ø
302536
Askenbom Ingrid A.
Hellsten Karl M.e.
Klingberg Anders W.
Berol Kemi Ab
Macrae & Co.
LandOfFree
Process for the concentration of sulfidic nickel ores does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for the concentration of sulfidic nickel ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the concentration of sulfidic nickel ores will most certainly appreciate the feedback.