Abstract In the disclosed two stage process for the delignification of cellulose containing raw materials, the extraction is carried out with aqueous acetic acid at a temperature of 140 to 230°C and a pressure of 3 to 30 bar with a subsequent extraction or washing. The obtained acetic acid wet cellulose is subsequently treated with an ozone containing gas. The use of halogenous additives or bleaching agents is no longer required. The process provides for a residual lignin content of less than 1% per weight, even if the yielded cellulose was extracted from coniferous wood which is hard to delignify,

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for the delignification of cellulose containing raw... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the delignification of cellulose containing raw..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the delignification of cellulose containing raw... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2070879

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.