Abstract Process for the manufacture of coarse aluminum hydroxide, con- taining a maximum of 15 weight percent of the particles in a par- ticle size under 45 micrometres, with a productivity that may be higher than 60 grams of precipitated Al203. The process consists of a decomposition in two stages (an agglo- meration phase and a growth phase); each stage proceeding within defined temperature ranges with seed material of different con- stitution. The first (fine) seed amount is added at the start of the decomposition in such an amount, that the ratio of the super- saturation of the aluminate liquor to the surface area of the seed position exhibits a value of 7 to 25 grams per square metre. The process exhibits the advantage of the high productivity of the so- called European process and the advantage of the so-called American process by obtaining a coarse product hydroxide. -1-

339243

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for the manufacture of coarse aluminum hydroxide does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the manufacture of coarse aluminum hydroxide, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the manufacture of coarse aluminum hydroxide will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-562287

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.