Process for the production of high molecular weight...

C - Chemistry – Metallurgy – 08 – G

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C08G 63/20 (2006.01) B29B 7/46 (2006.01) C08G 63/80 (2006.01) B29C 47/00 (2006.01)

Patent

CA 2096640

Preparation of high molecular weight polyester resins starting from resins with intrinsic viscosity I.V. lower than 0.57 dl/ comprising the following steps: (1) mixing the resin in the melt with a polyaddition additive containing at least two groups cap- able of addition reactions with the terminal OH and COOH groups of the resin; (2) converting the melted polyester into solid particles and then subjecting the particles to crystallization; (3) heating the particles at temperature between 150 and 210 °C up~ obtain the desired increase of intrinsic viscosity.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for the production of high molecular weight... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the production of high molecular weight..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of high molecular weight... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1785505

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.