ABSTRACT OF THE DISCLOSURE Zinc, copper and cadium are recovered from their ferrites by subjecting the ferrites to a sulfuric acid bearing solution in the presence of potassium, sodium or ammonium ions under atmospehric conditions at 80-105°C to precipitate the iron present in the ferrites as jarosite, separating at least a portion of the jarosite-bearing solid material from the solution before recycling the solution to a neutral leach, from which a copper and cadium bearing solution is recovered and to which acid and clacine are also fed, feeding the solid obtained from the neutral leach to the said ferrite treatment stage classifying the solid obtained from the neutral leach into a finer and coarser fraction, feeding the finer fraction to the ferrite treatment stage, comminuting the coarser fraction by grinding, leaching or milling and recycling the comminuted fraction to the process.

309320

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for the recovery of zinc, copper and cadmium in the... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the recovery of zinc, copper and cadmium in the..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the recovery of zinc, copper and cadmium in the... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-411097

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.