Abstract of the Disclosure A process of producing a fiber-reinforced hardened body of gypsum system comprises mixing gypsum and slag in a ratio by weight of the former to the latter between 3 : 7 and 7 : 3 to prepare a main starting material, adding to the main starting material 1 - 30% by weight of reinforcing fiber, 0.1 - 5% by weight of alkali salt substance, and 0.1 - 5% by weight of aluminum sulfate-containing substance, the respective amounts being based on the weight of the main starting material, further adding water to knead and mold the resulting starting material mixture, and curing the molded starting material mixture under normal con- dition or steam-curing tho molded starting material mixture at 90°C or below.

323662

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process of producing fiber-reinforced hardened body of... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process of producing fiber-reinforced hardened body of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of producing fiber-reinforced hardened body of... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-193467

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.