ABSTRACT OF THE DISCLOSURE Process of sulfurizing a blend of 90 to 50 and prefer- ably 88 to 70 parts by volume of triglyceride such as lard oil and 10 to 50 and preferably 12 to 30 parts by volume of an ethylenically unsaturated hydrocarbon containing 2 to 24 carbon atoms. The sulfurization is carried out using elemental sulfur. Simultaneous sulfurization and chlorination may be effected by reacting with sulfur monochloride. Phosphosulfurization may also be carried out by addition of small amounts of a phosphorus sulfide to the sulfurized blend followed by heating at 180°F. to 250°F. for from 30 minutes to 10 hours to effect phosphosulfuri- zation. The sulfurization or phosphosulfurization involves react- ing at from 330°F. to 445°F. for 20 minutes to 10 hours followed by blowing with a gas at from 125°F. to 250°F. for 30 minutes to 20 hours to remove hydrogen sulfide. The simultaneous sulfuriza- tion and chlorination reaction is carried out at from 90°F. to 280°F. for from 20 minutes to 10 hours followed by blowing with a gas at from 125°F. to 250°F for 30 minutes to 20 hours. The sulfurized oils contain from 7.5 to 25 weight percent sulfur as based on the blend of olefin and triglyceride.
134156
Gowling Lafleur Henderson Llp
Sun Research And Development Company
LandOfFree
Process of sulfurizing lard oil and an olefin and resultant... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process of sulfurizing lard oil and an olefin and resultant..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of sulfurizing lard oil and an olefin and resultant... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1289021