ABSTRACT In the rolling mill the temperature of the product is reduced to between Ac3 and Ac3 + 150°C before it enters the finishing stands. The product emerging from the finishing stands is quenched to provide a surface layer of martensite and/or bainite. Subsequently the heat of the core of the product is allowed to raise the temperature of the surface layer to between 450 and 750°C, so that the quenched layer is tempered.
244523
Economopoulos Mario
Respen Yves J.
LandOfFree
Producing rolled steel products does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Producing rolled steel products, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Producing rolled steel products will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-527929