CA 1072296
ABSTRACT OF DISCLOSURE A method of making elongate cubic boron nitride particles including the steps of providing a reaction zone, placing in the reaction zone a sleeve of hexagonal boron nitride around a core of catalyst for cubic boron nitride formation, the weight ratio of hexagonal boron nitride to catalyst being in the range 10:1 to 3:1 and the catalyst being selected from alkali metals, alkaline earth metals and nitrides thereof and subjecting the contents of the: reaction zone to conditions of temperature and pressure suitable for cubic boron nitride formation. This method produces novel cubic boron nitride particles which are characterised by a long axis and a short transverse axis, the ratio of the long axis to the short axis being at least 3 : 1 and the long axis being in the <111> crystallographic direction.
231085
LandOfFree
Production of cubic boron nitride does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Production of cubic boron nitride, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Production of cubic boron nitride will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-83479