C - Chemistry – Metallurgy – 22 – C
Patent
C - Chemistry, Metallurgy
22
C
C22C 1/02 (2006.01) C22C 1/03 (2006.01) C22C 21/00 (2006.01) C22F 1/04 (2006.01) C22F 3/00 (2006.01)
Patent
CA 2361484
A method of controlling grain size in as-cast aluminum alloy having the steps of a) providing a molten aluminum alloy including an alloying element selected from the group consisting of Ti, Sc, Zr, V, Hf, Nb and Y; b) adding a grain refiner to the molten aluminum alloy to form a melt; and c) solidifying the melt to form an ingot. The grain refiner includes Ti and B or C, and is added to the melt in an amount to yield the concentration in the melt of B or C from the grain refiner of about 0.003-0.010 wt. %. Grains in the as-cast aluminum alloy are about 200 microns or less in size.
Alcoa Inc.
Smart & Biggar
LandOfFree
Production of ultra-fine grain structure in as-cast aluminum... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Production of ultra-fine grain structure in as-cast aluminum..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Production of ultra-fine grain structure in as-cast aluminum... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1801318