IMPROVED AND PROPERTY-BALANCED NICKEL-BASE SUPERALLOYS FOR PRODUCING SINGLE CRYSTAL ARTICLES ABSTRACT The present invention is directed to the achievement of increased gas turbine engine efficiencies through futher improvements in nickel-base superalloys used to make parts and components for gas turbine engines. The present invention comprises nickel-base superalloys for producing single crystal articles having a significant increase in temperature capability, based on stress rupture strength and low and high cycle fatigue proprieties over single crystal articles made from current production nickel-base superalloys. Further, because of their superior resistance to degradation by cyclic oxidation, and their resistance to hot corrosion, the superalloys of this invention possess a balance in mechanical and environmental properties which is unique and has not heretofore been obtained.
533975
Buchakjian Leo Jr.
Wukusick Carl Stephen
Company General Electric
Craig Wilson And Company
LandOfFree
Property-balanced nickel-base superalloys for producing... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Property-balanced nickel-base superalloys for producing..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Property-balanced nickel-base superalloys for producing... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1191446