A method is disclosed for recovering the properties of single crystal and directionally solidified Nickel based superalloys and articles made thereof, after use in a high temperature environment. The method comprises the steps of a stress relief treatment, a .gamma.' rejuvenation heat treatment at a temperature below the .gamma.'-solvus temperature (Tsolvus, .gamma.) of the superalloy, a precipitation heat treatment and an aging heat treatment.

L'invention concerne un procédé permettant de restaurer les propriétés de superalliages à base de nickel monocristallin et à orientation dirigée, et d'articles faits à partir de ceux-ci, après leur utilisation dans un environnement à haute température. Le procédé comporte les étapes consistant à mettre en oeuvre : un traitement de recuit de détente ; un traitement thermique de rajeunissement ?' à une température inférieure à la température de solubilité ?' (T¿solubilité?, ¿?'?) du superalliage ; un traitement thermique de précipitation et un traitement thermique de vieillissement.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Property recovering method for nickel superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Property recovering method for nickel superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Property recovering method for nickel superalloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2012555

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.