ABSTRACT OF THE DISCLOSURE A means for using "workable-weldable" austenitic stainless steel in an environment where stress corrosion cracking would have been a problem. The austenitic stainless steel is protected against stress corrosion cracking by covering a portion thereof with another stainless steel which is less noble than the austenitic steel in the referred to corrosive environment.
328401
Johnson Mark J.
Lula Remus A.
Pavlik Paul J.
Allegheny Ludlum Corporation
George H. Riches And Associates
LandOfFree
Protecting austenitic stainless steel from stress corrosion... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Protecting austenitic stainless steel from stress corrosion..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Protecting austenitic stainless steel from stress corrosion... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-299870