CA 2534282
Pour protéger contre la corrosion un superalliage monocristallin riche en rhénium tout en évitant la formation de zones de réaction secondaire évolutives, on dépose sur sa surface, avant un traitement d'aluminisation, une couche (3) constituée de tungstène et de cobalt.