ABSTRACT OF THE DISCLOSURE A process for recovering cobalt and nickel values from cobalt and nickel containing sulphidic material also containing iron includes roasting the sulphidic material to produce a calcine containing water soluble cobalt and nickel sulphate, and leaching the calcine in aqueous sulphate solu- tion under oxidizing conditions at an oxygen overpressure in the range of from about 50 kPa to about 1500 kPa and at a temperature in the range of from about 100 to about 180°C to produce an iron-containing residue and a cobalt and nickel containing solution. The residue is separated from the solution, and cobalt and nickel values are recovered from the solution.
424733
Chalkley Michael E.
Kerfoot Derek E.
Weir Donald R.
Gowling Lafleur Henderson Llp
Sherritt International Consultants Inc.
LandOfFree
Recovery of cobalt and nickel from sulphidic material does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Recovery of cobalt and nickel from sulphidic material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Recovery of cobalt and nickel from sulphidic material will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1274990