Refractory mix composition and method of preparation

C - Chemistry – Metallurgy – 04 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

261/36, 261/66

C04B 35/18 (2006.01) C04B 28/34 (2006.01) C04B 35/101 (2006.01)

Patent

CA 1093103

ABSTRACT OF THE DISCLOSURE The invention relates to an alumina based, phosphate bondable, dry refractory mix composition exhibiting an extended shelf life of up to eighteen months and longer. The mixture has the following preferred composition on a weight percentage basis: 40-70% sized tabular alumina, 15-35% calcined alumina, 2-10% hydrated alumina, 1-10% calcium aluminate cement and an acid ingredient such as 3 to 15 weight percent of a 115 percent concentration of polyphosphoric acid. The mix is prepared by a method which comprises the steps of formulating dry ingredients into a mixer, mixing the dry ingredients to a homogenous state, then adding a liquid acid ingredient to the mixture of dry ingredients, and subjecting the dry and acid ingredient mix to a high intensity mixing action for a predetermined period of time. The product is substantially dry to the touch.

306917

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Refractory mix composition and method of preparation does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Refractory mix composition and method of preparation, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Refractory mix composition and method of preparation will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-992052

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.