ABSTRACT A sulphur-bituminous composite material consisting essentially of 60-75% by weight sulphur and 25-40% by weight bituminous material, and optionally containing a small amount of a fibrous or flake reinforcing material and usually with a filler which is suitable for use as a self- compacting road or pothole repair material. A feature of the composite is the presence of two continuous phases in the composite which is achieved either by mixing solid particulate sulphur with a softened bituminous material at a temperature in the range 120-150°C or by mixing liquid sulphur with liquid bituminous material with a sufficient shearing-mixing action to disperse the liquid sulphur as an emulsion with the bituminous material 80 as to provide on cooling a continuous, rigid, crystalline and porous sulphur skeleton in the composite.

237678

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Reinforced sulphur-asphalt composites does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Reinforced sulphur-asphalt composites, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Reinforced sulphur-asphalt composites will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-53911

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.