Roast-reductive leach process for copper recovery

C - Chemistry – Metallurgy – 22 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

53/286

C22B 15/00 (2006.01) C22B 23/00 (2006.01)

Patent

CA 1091036

ABSTRACT OF THE DISCLOSURE: A sulfide containing copper and one or more of iron, nickel and cobalt, is dead-roasted at a temperature of 750°C or above, then subjected to a pressure leach under reducing conditions to produce elemental copper and an aqueous solution of the other metals.

278360

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Roast-reductive leach process for copper recovery does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Roast-reductive leach process for copper recovery, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Roast-reductive leach process for copper recovery will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-477034

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.