SELENIUM REJECTION DURING ACID LEACHING OF MATTE Abstract of Disclosure A method is provided for removing trace amounts of selenium from acid leach solutions containing over 2 ppm of total selenium comprising either Se(IV) and/or Se(VI) obtained during the pressure oxidation leaching of metal sulfide con- centrate comprising forming a slurry of said acid solution with comminuted metal sulfide concentrate, said slurry con- taining at least two grams of a metal ion as metal hydroxide per liter of solution and then subjecting said slurry to agi- tation at a temperature of at least about 185°C at a pressure of at least about 160 psig, whereby to reduce the total sele- nium content of said solution to less than about 2 ppm.

246459

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Selenium rejection during acid leaching of matte does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Selenium rejection during acid leaching of matte, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Selenium rejection during acid leaching of matte will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-642654

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.