CA 2550787
A method of laser beam welding at least two adjacent superalloy components (12, 14) includes (a) aligning the components along a pair of faying surfaces (18, 20) but without a backing plate; (b) placing a superalloy shim (16) between the faying surfaces; (c) welding the components together using a laser beam causing portions of the superalloy components along the faying surfaces to mix with the superalloy shim; and cooling the components to yield a butt weld (22) between the components.
Feng Ganjiang
Nowak Daniel Anthony
Spiegel Lyle B.
Company General Electric
Craig Wilson And Company
LandOfFree
Shimmed laser beam welding process for joining superalloys... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Shimmed laser beam welding process for joining superalloys..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Shimmed laser beam welding process for joining superalloys... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-2052334