CA 1249724
ABSTRACT OF THE DISCLOSURE The present invention relates to a Weak Pre-Deoxida- tion Process (abbreviated as W.P.D. process) for producing Al- killed and/or Ti-Killed steel. In this process the proper amount of Si-containing ferro-alloy is added into molten steel during tapping, as Weak Pre-Deoxidation, then the ladle is transferred to Al-Wire feeder system or ladle injection treat- ing equipment to proceed final stage of deoxidation. Not only can the recovery rate of deoxidizer be increased by this new process, but also the cleanliness as well as surface and inter- nal quality of products are effectively improved. Besides, the production cost will be reduced due to less deoxidizer addition, less billet conditioning cost, less rejection and less customer claim. Thus the W.P.D. process is a break-through in present steelmaking practice.
477155
Jin-Luh Su
Li-Jung Hu
Maw-Cheng Shieh
Seng-Jung Chen
China Steel Corporation
Hewitt Neville S.
LandOfFree
Si contained ferroalloy addition as a weak pre-deoxidation... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Si contained ferroalloy addition as a weak pre-deoxidation..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Si contained ferroalloy addition as a weak pre-deoxidation... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1307375