Abstract of the disclosure: Mixtures which are used for the production ofof polyurethane foam and which contain amines having primary or secondary aliphatic hydroxyl groups, and also custom- ary quantities of trichlorotrifluoroethane and/or tri- chlorofluoromethane as a blowing agent, can be stabilized against the premature reaction of the components by add- ing 0.05 to 5% by weight of 2,4-diphenyl-4-methylpentene in which the ratio of the 2,4-diphenyl-4-methyl-1-pentene isomer to the 2,4-diphenyl-4-methyl-2-pentene isomer is 1:1 to 9:1, the percentages relating to the chlorofluoro- alkane. In particular, these mixtures can be stabilized by adding 0.1 to 5% by weight of a mixture consisting of 45 to 89% by weight of 2,4-diphenyl-4-methyl-1-pentene, 10 to 45% by weight of 2,4-diphenyl-4-methyl-2-pentene and 1 to 20% by weight of 1,1,3-trimethyl-3-phenylindane.
412709
Behme Klaus-Jurgen
Hoffmann Bernd
Fetherstonhaugh & Co.
Hoechst Aktiengesellschaft
LandOfFree
Stabilization of polyether or polyester molding compositions... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Stabilization of polyether or polyester molding compositions..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Stabilization of polyether or polyester molding compositions... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1318229