- 12 - Stress Corrosion Resistant Al-Mg-Li-Cu Alloy Abstract An aluminum base alloy having a composition within the following ranges in weight per cent:- Lithium - 2.1 - 2.9 Magnesium - 3.0 - 5.5 Copper - 0.2 - 0.7 and one or more constituents selected from the group consisting of Zirconium, Hafnium and Niobium as follows:- Zirconium - 0.05 - 0.25 Hafnium - 0.10 - 0.50 Niobium - 0.05 - 0.30 and Zinc - 0 - 2.0 Titanium - 0 - 0.5 Manganese - 0 _ 0.5 Nickel - 0 - 0.5 Chromium - 0 _ 0.5 Germanium - 0 - 0.2 Aluminum - Remainder (apart from incidental impurities)
465106
Gray Alan
Miller William S.
British Aluminium Limited
Sim & Mcburney
LandOfFree
Stress corrosion resistant al-mg-li-cu alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Stress corrosion resistant al-mg-li-cu alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Stress corrosion resistant al-mg-li-cu alloy will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1268328