CA 2076091

13DV-8682 SUPERALLOY COMPONENT WITH DISPERSION-CONTAINING PROTECTIVE COATING, AND METHOD OF PREPARATION ABSTRACT OF THE DISCLOSURE A coated superalloy component includes a substrate article formed of a superalloy and an adherent coating over the substrate. The coating is a nickel-base superalloy containing at least about 0.3 volume percent or more of a dispersed oxide of yttrium, hafnium and/or a rare earth, and, preferably, grain boundary strengthening elements such as carbon, zirconium, and boron. The oxide dispersoids improve the performance of the coating in service, reducing the incidence failures due to thermal fatigue, oxidation, and corrosion damage. The dispersoid-containing coating may be formed by directly depositing the oxide-containing coating, or by depositing a metallic coating and then forming the dispersoids by subsequent heat treatment.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Superalloy component with dispersion-containing protective... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Superalloy component with dispersion-containing protective..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy component with dispersion-containing protective... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1730871

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.