SUPERALLOY COMPOSITION AND PROCESS ABSTRACT OF THE DISCLOSURE A nickel superalloy composition and process for producing novel, high strength articles of the alloy are described. The composition is based on the Ni-Al-Mo system. Outstanding properties are obtained by producing the alloy in powder form, compacting the powder and causing directional secondary recrystallization in the compacted powder. The resultant articles have high temperature properties which are superior to those of known commercial superalloys. F-4237
324088
Bourdeau Romeo G.
Cox Arthur R.
Swabey Ogilvy Renault
United Technologies Corporation
LandOfFree
Superalloy composition and process does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy composition and process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy composition and process will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-20763