CA 2401970

A high velocity oxygen fuel thermal spray powder comprising a superalloy having the formula MCrAlY-X, wherein M is at least one metal taken from the group consisting of nickel, cobalt, and iron; X is at least one reactive element taken from the group consisting of hafnium, rhenium, lanthanum, and tantalum; and yttrium is present in levels greater than 1 % by weight of the total composition and up to about 6 % by weight of the total composition. In addition, the powder may be blended with an agglomeration of M'CrAlY and a ceramic, wherein M' is at least one metal taken from the group consisting of nickel, cobalt, and iron. The invention offers improved high temperature oxidation, corrosion and creep resistance.

L'invention porte sur une poudre thermique pulvérisable du type HVOF (High Velocity Oxygen Fuel) consistant en un superalliage de formule MCrAlY-X, dans laquelle: M est au moins un métal choisi parmi Ni, Co et Fe; X est au moins un élément réactif choisi parmi Hf, Re, La et Ta, et Y est de 1 6 % en poids de la composition totale, d'yttrium. Ladite poudre peut de plus être mélangée à un aggloméré de céramique et de M'CrAlY, formule dans laquelle M' est au moins un métal choisi parmi Ni, Co et Fe. Ladite poudre présente une meilleure résistance à l'oxydation, à la corrosion et au fluage à haute température.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Superalloy hvof powders with improved high temperature... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Superalloy hvof powders with improved high temperature..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy hvof powders with improved high temperature... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1704211

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.