CA 2545863
A method for forming or remanufacturing a component to have an internal space. A refractory metal blocking element is formed, in situ, with at least a portion to be within the internal space. The formation includes an at least partial melting. A material is added, the blocking element at least partially blocking entry of the material to the internal space. The blocking element is removed.
Finn John H.
Moor James J.
Szela Edward R.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
United Technologies Corporation
LandOfFree
Superalloy repair methods does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy repair methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy repair methods will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1395473