B23P 6/00 (2006.01) B21D 51/00 (2006.01) B23K 3/08 (2006.01) B23K 26/34 (2006.01) B23K 26/42 (2006.01) B23K 35/38 (2006.01) B23P 15/02 (2006.01) B21D 53/78 (2006.01)
Patent
CA 2545634
A method for forming or remanufacturing a component to have an internal space. A refractory metal blocking element is formed, in situ, with at least a portion to be within the internal space. A material is added by at least one of welding, laser cladding, and diffusion brazing, the blocking element at least partially blocking entry of the material to the internal space. The blocking element is removed.
Pietruska Norman
Szela Edward R.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
United Technologies Corporation
LandOfFree
Superalloy repair methods and inserts does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy repair methods and inserts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy repair methods and inserts will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1451496