ABSTRACT OF THE DISCLOSURE Cold-worked superalloys having improved resistance to hydrogen embrittlement are disclosed. These new superalloys are nickle- or cobalt-chromium-molyb- denum superalloys and possess improved resistance to hydrogen embrittlement rendering them useful in deep sour gas wells.
322028
Berkowitz Barry J.
Kane Russell D.
Borden Ladner Gervais Llp
Exxon Production Research Company
Exxon Research And Engineering Company
LandOfFree
Superalloys having improved resistance to hydrogen... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloys having improved resistance to hydrogen..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloys having improved resistance to hydrogen... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-996168