Synthesis of a crystalline silicoaluminophosphate

C - Chemistry – Metallurgy – 01 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

252/2.C, 260/675

C01B 37/08 (2006.01) B01J 29/04 (2006.01) B01J 29/85 (2006.01)

Patent

CA 1253838

SYNTHESIS OF A CRYSTALLINE SILICOALUMINOPHOSPHATE ABSTRACT A method for the synthesis of the silicoaluminophosphate SAPO-37 comprises preparing a two-phase reaction mixture containing the required starting materials divided between a liquid organic phase and a liquid aqueous-phase. The reaction mixture is then heated at a rate of from 5°C to 200°C per hour to a temperature of from 80°C to 200°, while being agitated in a manner sufficient to intimately admix the liquid organic and aqueous phases. Once nucleation of the silicoaluminophosphate occurs the agitated reaction mixture is heated at rate of from 5°C to 200°C per hour to a temperature of from 100°C to 300° and maintained then at the higher temperature and at a pH of from 2 to 9 until crystals of the desired silicoaluminophosphate are formed.

496558

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Synthesis of a crystalline silicoaluminophosphate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Synthesis of a crystalline silicoaluminophosphate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Synthesis of a crystalline silicoaluminophosphate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1212624

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.