B32B 15/04 (2006.01) C23C 14/08 (2006.01) C23C 28/00 (2006.01)

Patent

CA 2165932

A ceramic thermal barrier coating coating (14) for superalloy articles (10) is caused to adhere more strongly to an aluminium-containing alloy bond coating (13) by diffusing platinum into the bond coating (13) so as to ensure formation of a platinum rich outer layer (20) of the bond coating (12a), including a platinum aluminide surface layer (22) of the bond coating (12a), and by subsequent formation of a thin coherent layer (16a) of alumina between the platinum aluminide surface layer (22) and the ceramic coating (14), which reduces the tendency of the ceramic coating (14) to spall during service.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Thermal barrier coating for a superalloy article and method... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Thermal barrier coating for a superalloy article and method..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermal barrier coating for a superalloy article and method... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1402282

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.