ABSTRACT Provided is an improved aluminum-titanium master alloy contain- ing carbon in a small but effective content and not more than about 0.1%. After melting, the master alloy is superheated to about 1200-1250°C to put the carbon into solution, then the alloy is cast in a workable form. The master alloy in final form is substantial- ly free of carbides greater than about 5 microns in diameter. The alloy of this invention is used to refine aluminum products that may be rolled into thin sheet, foil, or fine wire and the like.
546157
Gowling Lafleur Henderson Llp
Kb Alloys Llc
LandOfFree
Third element additions to aluminum-titanium master alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Third element additions to aluminum-titanium master alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Third element additions to aluminum-titanium master alloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1217996