ABSTRACT OF THE DISCLOSURE This is a process for producing improved chlor- ide corrosion resistance in turbine components fabricated from stainless steels which contains generally at least 1% if both a martensitic and metastable austenitic phase and comprises an initial high-intensity shot peening, followed by an aging cycle at about 980-1020°F for ?-4 hours and a final (lower intensity) shot peening. A relatively homogeneous surface of aged marten- site is produced and selective attack which forms sharp pit-like defects which initiate cracks is avoided.
402682
Oldham And Company
Westinghouse Electric Corporation
LandOfFree
Three-step treatment of stainless steels having metastable... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Three-step treatment of stainless steels having metastable..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Three-step treatment of stainless steels having metastable... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1288789