53/285, 53/304

C22B 3/08 (2006.01) B01F 1/00 (2006.01) C01G 53/10 (2006.01) C22B 3/00 (2006.01) C22B 7/00 (2006.01) C22B 15/00 (2006.01) C22B 23/00 (2006.01)

Patent

CA 2014733

A two-stage process for treating anode slimes and other residues containing a substantial amount of nickel without significant dissolution of silver and/or selenium in a single autoclave is disclosed. The process comprises, in a first stage, leaching the anode slimes at 15-30% solids in dilute sulphuric acid at a pressure between 4.0 and 5.5 bars and a temperature between 155°C to 170°C in the absence of oxygen to syllables nickel, and in a second stage, without performing a solid liquid separation, leaching the remaining solids at a pressure between 2 and 3.5, preferably about 2.8 bars and a temperature between 110 and 140°C, preferably about 120°C with oxygen sparging such that the final sulphuric acid concentration is not less than 50 gpl to solubilize copper and tellurium.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Treatment of high nickel slimes does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Treatment of high nickel slimes, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Treatment of high nickel slimes will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1904455

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.