ABSTRACT A novel nickel-base high temperature alloy body preferably containing about 22% chromium, sufficient aluminum and titanium to provide a ? precipitate structure, additional strengthing elements and oxidic yttrium in finely dispersed form. The alloy body has an elongated crystal structure and is characterized by high strength along with excellent hot corrosion and oxidation resistance.
503715
Andryszak Kenneth R.
Benn Raymond C.
Davidson Jeffrey M.
Inco Alloys International Inc.
Smart & Biggar
LandOfFree
Turbine blade superalloy i does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Turbine blade superalloy i, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Turbine blade superalloy i will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1323126