CA 1255123
ABSTRACT A novel, nickel-base, high temperature alloy body preferably containing about 20% chromium, 6 to 7% aluminum to provied ? phase, 1.5 to 2.5% molybdenum, 3 to 4.5% tungsten, additional strengthening elements and oxidic yttrium in finely dispersed form. The alloy body has an elongated crystal structure and is characterized by high strength along with excellent hot corrosion and oxidation resistance.
503724
Andryszak Kenneth R.
Benn Raymond C.
Davidson Jeffrey M.
Inco Alloys International Inc.
Smart & Biggar
LandOfFree
Turbine blade superalloy ii does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Turbine blade superalloy ii, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Turbine blade superalloy ii will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1212351