C - Chemistry – Metallurgy – 30 – B
Patent
C - Chemistry, Metallurgy
30
B
75/3
C30B 11/14 (2006.01) B22D 25/06 (2006.01) B22D 27/04 (2006.01) C30B 11/00 (2006.01)
Patent
CA 981487
Giamei Anthony F.
Kear Bernard H.
Tschinkel Johann G.
LandOfFree
Unidirectionally solidified superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Unidirectionally solidified superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Unidirectionally solidified superalloy articles will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-172546