ABSTRACT OF THE DISCLOSURE The present invention provides a process of upgrading the nickel from nickel lateritic iron ore with iron content over 10%, silica content over 25% and nickel content of at least 0.5% which process comprises thoroughly mixing the ground ore with calcium carbonate, calcium sulphate and coke, spraying the mixture with a solution of sodium chloride, drying the mixture, heating the mixture at a temperature not exceeding 1050° C, for a period of time up to 90 minutes, roasting the mixture at the above temperature for a sufficient period of time to convert all nickel in the ore to metallic state in a neutral or even slightly reducing atmosphere, grinding the roasted mixture in an aqueous medium, and adjusting the density of the pulp obtained for a subsequent flotation or by magnetic separation process to produce a concentrate.
249487
LandOfFree
Upgrading the nickel content from low grade nickel lateritic... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Upgrading the nickel content from low grade nickel lateritic..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Upgrading the nickel content from low grade nickel lateritic... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1137756