CA 1302741
ABSTRACT Problems are caused by stress corrosion cracking and exfoliation cracking in the heat-affected zones adjacent welds in structure of welded components formed of Al alloys, particularly of the 7000 series but also of the 5000 series. The invention seeks to overome these by the use of Al-Mg welding wire containing 0.01- 0.5% Ga and/or In and/or Sn, the composition being chosen such that the weld bead has a potential at least as electronegative as the components and preferably in the range -1200 to -1130 mV with reference to a standard calomel electrode. To prevent diffusion of Ga/In/Sn, the components may be pre-coated eg by using a double-pass welding technique.
547889
Hepples Warren
Holroyd Nigel John Henry
Scamans Geoffrey Mark
British Aluminium Limited
Fetherstonhaugh & Co.
LandOfFree
Welding aluminium alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Welding aluminium alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Welding aluminium alloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1261712