75/53, 148/35.7

C22C 16/00 (2006.01) C22F 1/18 (2006.01) G21C 3/07 (2006.01)

Patent

CA 2024068

This is an alloy comprising, by weight percent, 0.5-2.0 niobium, 0.7-1.5 tin, 0.07-0.14 iron, and 0.03- 0.14 of at least one of nickel and chromium, and at least 0.12 total of iron, nickel and chromium, and up to 220 ppm C, and the balance essentially zirconium. Preferably, the alloy contains 0.03-0.08 chromium, and 0.03-0.08 nickel. The alloy is also preferably subjected intermediate recrystallization anneals at a temperature of about 1200- 1300°F, and to a beta quench two steps prior to final size.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Zirconium alloy for light water reactor applications does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Zirconium alloy for light water reactor applications, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Zirconium alloy for light water reactor applications will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1377664

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.