9/17

D21C 3/02 (2006.01) D21C 3/26 (2006.01)

Patent

CA 1080914

PULPING OF HARDWOOD WITH SODIUM SULFIDE AND SODIUM HYDROXIDE WHILE GENERATING HYDROGEN SULFIDE IN SITU IN THE INITIAL PULPING STAGES ABSTRACT OF THE DISCLOSURE A process is provided for pulping hardwood,producing cellulose pulp in good yield and of high quality, with a low requirement for causticized pulping liquor, which comprises in a first pulping stage pulping the hardwood in an alkaline pulping liquor containing sodium sulfide at a temperature within the range from about 110 to about 170°C while generating hydrogen sulfide in situ by reaction of sodium sulfide with organic acids liberated in the pulping; and then in a second pulping stage following directly after the first pulping stage, continuing the pulping at a higher temperature within the range from about 145 to about 190°C in the presence of an alkaline pulping liquor comprising sodium hydroxide and a sodium sulfide until cellulose pulp is produced.

271114

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Pulping of hardwood with sodium sulfide and sodium hydroxide... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Pulping of hardwood with sodium sulfide and sodium hydroxide..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pulping of hardwood with sodium sulfide and sodium hydroxide... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-11152

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.