ABSTRACT Lead bismuth and tellurium and/or sulfur are added to steel, to increase the machinability of the steel, in an addition alloy consisting essentially of 5-40 parts lead, 5-40 parts bismuth, up to 6 parts tellurium and up to 25 parts sulfur. The alloy contains at least one of the group tellurium and sulfur, and the alloy has a melting point of at least about 400°C (752°F).

347994

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method and alloy for introducing machinability increasing... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method and alloy for introducing machinability increasing..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and alloy for introducing machinability increasing... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-111991

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.