Lead that forms dross upon melting is refined by treatment with refining agents consisting essentially of calcium metal and aluminum-silicon eutectic alloy. The refining agents are mixed into a bath of molten lead preferably at 600°C, the bath is cooled to preferably 450°C, and sodium hydroxide and sodium nitrate are added to remove the refining agents. The formed dross is skimmed and refined lead is recovered. The refined lead forms less dross upon remelting.

609401

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for the refining of lead does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for the refining of lead, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the refining of lead will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1322174

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.