Thermoelectic material and process for manufacturing the same

B - Operations – Transporting – 22 – F

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

B22F 9/04 (2006.01) B22F 1/00 (2006.01) C04B 35/547 (2006.01) C04B 35/645 (2006.01) C22C 1/05 (2006.01) H01L 35/00 (2006.01) H01L 35/28 (2006.01) H01L 35/34 (2006.01)

Patent

CA 2418994

A thermoelectric material is prepare by mixing and melting at least two members selected from bismuth, tellurium, selenium, antimony, and sulfur to obtain an alloy ingot; grinding the alloy ingot to obtain powder of the alloy ingot; and hot pressing the powder of the alloy ingot. The hot pressing is performed under the conditions of a temperature of 500°C or higher and 600°C or lower and a pressure of 20 MPa or higher and 45 MPa or lower.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Thermoelectic material and process for manufacturing the same does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Thermoelectic material and process for manufacturing the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Thermoelectic material and process for manufacturing the same will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1616222

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.