C08L 77/00 (2006.01) C08L 23/02 (2006.01) C08L 23/08 (2006.01) C08L 51/04 (2006.01) C08L 51/06 (2006.01) C08L 23/10 (2006.01) C08L 23/16 (2006.01)

Patent

CA 2123080

2123080 9309183 PCTABS00022 A process for melt-blending a polyamide with a crystalline polyolefin incompatible therewith in the presence of a rubbery compatibilizing polymer capable of chemically or physically associating with both the polyamide and the polyolefin, at a process temperature higher than the highest melting temperature of any crystalline polymer present and higher than the highest glass transition temperature of any amorphous polymer present but such that significant degradation of any polymer present does not occur, all blend components being present within stated ranges, and the melt viscosity ratio of the polyamide to that of the polyolefin at the process temperature and a shear rate of about 100-200 sec-1 being about 0.1-1.2, especially 0.4-0.8. High stiffness, supertough polymer blends, where notched Izod impact strength exceeds 535 J/m, are obtained.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for making polyamide/polyolefin blends having... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making polyamide/polyolefin blends having..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making polyamide/polyolefin blends having... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1825281

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.