ABSTRACT OF THE DISCLOSURE A process for improving the elongation of copper base alloys containing about 2 to 4.5% aluminum, 15 to 31% zinc, and a grain refining element such as iron, chromium, zirconium, or cobalt, is carried out through controlled grain coarsening. Such alloys are subjected to a cold reduction of about 15 to 40%, an intermediate anneal at about 625° to 725°C, a final cold reduction of 12 to 45% and a final anneal at about 600° to 725°C. Alternatively, the above sequence may be preceded by a preliminary cold reduction of about 10 to 70% and then a preliminary low temperature anneal at about 400° to 600°C followed by the above reductions and anneals.
239999
Crane Jacob
Shapiro Eugene
LandOfFree
Process for improving the elongation of grain refined copper... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for improving the elongation of grain refined copper..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for improving the elongation of grain refined copper... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-31811